Original price was: $458.14.$251.98Current price is: $251.98.
Fabric label, Roll, yellow (RAL 1018), unmarked, can be labeled with: THERMOMARK E.300 (D)/600 (D), THERMOMARK ROLL 2.0, THERMOMARK ROLL, THERMOMARK ROLL X1, THERMOMARK ROLLMASTER 300/600, THERMOMARK X1.2, mounting type: adhesive, Number of individual labels: 1000, text field height: 17 mm, text field width: 38 mm
| Minimum order quantity | 1 Piece |
| Packing unit | 1 Piece |
| Break packing | not allowed |
Available on backorder
Fabric label, Roll, yellow (RAL 1018), unmarked, can be labeled with: THERMOMARK E.300 (D)/600 (D), THERMOMARK ROLL 2.0, THERMOMARK ROLL, THERMOMARK ROLL X1, THERMOMARK ROLLMASTER 300/600, THERMOMARK X1.2, mounting type: adhesive, Number of individual labels: 1000, text field height: 17 mm, text field width: 38 mm
| Product type | Device marker |
|---|---|
| Product property | Low restoring force |
| Marking | |
| Number of individual labels | 1000 |
| Number of individual labels per row | 2 |
| Identification technology | Thermal transfer |
| Width | 38.00 mm |
|---|---|
| Height | 17.00 mm |
| Depth | 0.15 mm |
| Text field | |
| Text field width | 38 mm |
| Text field height | 17 mm |
| Color | yellow (RAL 1018) |
|---|---|
| Material | PA |
| Base element material | PA |
| Components | free from silicone and halogen |
| Ambient conditions | |
| Ambient temperature (operation) | 0 °C … 125 °C |
|---|---|
| Recommended ambient temperature (storage/transport) | 23 °C |
| Recommended humidity (storage/transport) | 50 % (Storage in a dry and dark place in the original packaging is recommended) |
| Test for substances that would hinder coating with paint or varnish | |
| Testing for paint wetting impairment substances (LABS-conformity) | VW PV 3.10.7:2005-02 |
| Result | Test passed |
| Testing for paint wetting impairment substances (LABS-conformity) | VDMA 24364:2018-05 |
| Result | Test passed |
| Scratch resistance | |
| Specification | EN ISO 1518-1:2023 (following) |
| Requirements | ≥ 5 N |
| Result | Test passed |
| UV resistance | |
| Specification | DIN EN ISO 4892-2:2021-11 (following) |
| Result | Test passed |
| Test duration | 96 h |
| Procedure | Artificial irradiation. |
| Moisture heat storage | |
| Specification | IEC 60068-2-78:2012-10 (following) |
| Result | Test passed |
| Duration | 96 h |
| Temperature for testing | 40 °C |
| Relative humidity | 93 % |
| Temperature resistance | |
| Specification | ANSI/UL 969-2018:03 (following) |
| Test duration | 240 h |
| Rating 125 °C (150 °C) | Test passed |
| Wipe resistance of inscriptions | |
| Specification | DIN EN 61010-1 (VDE 0411-01):2020-03 |
| Specification | DIN EN 62208 (VDE 0660-511):2012-06 (in parts) |
| <i>n</i>-Hexane<br/>[CAS No. 110-54-3] | Test passed |
| Water + Petroleum ether<br/>[CAS No. 64742-82-1] | Test passed |
| Sodium hydroxide 0.1 mol/l<br/>[CAS No. 1310-73-2] | Test passed |
| Immersion in chemicals, oil & fuel | |
| Specification | ISO 175:2010 (following) |
| Test duration | 168 h |
| Saltwater (saturated 350 g/l)<br/>[CAS No. – ] | Test passed |
| Diesel<br/>[CAS No. 68476-34-6] | Test passed |
| IRM 901 | Test passed |
| IRM 902 | Test passed |
| IRM 903 | Test passed |
| Testing in a condensation changing climate in the presence of sulfur dioxide | |
| Specification | DIN EN ISO 22479:2022-08 |
| Result | Test passed |
| Procedure | Method B |
| Cycles | 2 |
| Salt spray test | |
| Specification | DIN EN IEC 60068-2-11 (VDE 0468-2-11):2022-10 |
| Result | Test passed |
| Test duration | 96 h |
| Wipe resistance | DIN EN 61010-1 (VDE 0411-1) |
|---|
| Mounting type | adhesive |
|---|
| Article Number | 0800557 |
|---|---|
| GTIN | 4046356606929 |
| Product Key | BG2411 |
| Status | Temporarily out of stock |
|---|---|
| Delivery | Expected to leave our warehouse in Canada on Jun 24, 2026, if ordered now |
| Estimated Delivery | Jun 24, 2026 |
| Ready to Ship | Jun 24, 2026 |
| Minimum Order Quantity | 1 Piece |
|---|---|
| Packing Unit | 1 Piece |
| Break Packing | Not allowed |